MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Cabot CABELEC® XS6560C PP, Conductive Compound
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product highlights: The CABELEC XS6560C conductive compound is a static dissipative compound made from carbon black dispersed in a polypropylene copolymer. Its electrical and mechanical properties are not dependent on atmospheric conditions. It has good rigidity and can be easily processed on conventional molding equipment.

Key applications: The CABELEC XS6560C conductive compound is suitable for use in applications where it is desirable to mitigate the hazard of electrostatic discharge, such as the molding of PP based conductive crates, pallets, and other plastic thick section applications. The static dissipative nature of the CABELEC XS6560C conductive compound provides products with a higher resistivity than typical conductive materials and can provide a long-lasting static dissipation.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Linear Mold Shrinkage 0.0030 cm/cmwidth; ASTM D955
 0.012 cm/cmlength; ASTM D955
Melt Flow 28 g/10 min
@Load 230 kg,
Temperature 5.00 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ISO 868
Tensile Strength at Break 21.0 MPaISO 527
Tensile Strength, Yield 26.0 MPaISO 527
Elongation at Break 15 %ISO 527
Flexural Modulus 1385 MPaISO 178
Izod Impact, Notched (ISO) 26.0 kJ/m²ISO 178
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 19000 ohm-cminjection molded plaque; IEC 61340-2-3
Surface Resistance <= 2.60e+6 ohminjection molded plaque; IEC 61340-2-3
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °CISO 75
Vicat Softening Point 151 °C
@Load 1.02 kg
ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 °Cbarrel
Nozzle Temperature 220 °C
Drying Temperature 90.0 °C
Dry Time 2.00 - 3.00 hour
 
Descriptive Properties
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT067 / 315802

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.