Toray PMC CFRT® (BW-1000/Reemay) is a reinforced thermoplastic composite laminate. It blends the benefits of a thermoplastic polymer matrix with woven carbon and glass fibers in a basket weave for enhanced shapes and performance. The BW-1000/Reemay style laminate is available in a dual-layer product; carbon in one direction and glass fibers in at a 90° orientation to carbon laminated over a layer of polyester fiber. The BW-1000/Reemay laminate is thin, lightweight, and resilient for improved energy return. Features: - Basket weave of carbon and glass fibers
- Bi-directional reinforcement with additional polyester fiber layer
- Lightweight, thin, dual-layer
- Available in various colors
Product Type And Composition: Carbon fiber content: 22%; Glass fiber content: 22%; Polyester fiber content: 9%; Modified PMMA thermoplastic resin: 47% (Nominal volume percentages) Typical Applications: - Footwear
- Recreational equipment
- Skates
Information provided by Toray Performance Materials Corporation. |