MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler

Material Notes: Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mechanical strength at elevated temperatures. Roving cloth in very coarse weave.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 - 1.90 g/cc1.70 - 1.90 g/ccIEC 1212-2 8.1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 300 MPa>= 43500 psiIEC 1212-2 5.7
Flexural Strength  >= 170 MPa
@Temperature 150 °C
>= 24700 psi
@Temperature 302 °F
Perpendicular to laminations; IEC 1212-2 5.1
 >= 340 MPa
@Temperature 23.0 °C
>= 49300 psi
@Temperature 73.4 °F
Perpendicular to laminations; IEC 1212-2 5.1
Flexural Modulus >= 20.0 GPa>= 2900 ksiIEC 1212-2 5.2
Compressive Strength >= 350 MPa>= 50800 psiPerpendicular to laminations; IEC 1212-2 5.3
Izod Impact, Unnotched (ISO) >= 54.0 kJ/m²>= 25.7 ft-lb/in²Parallel to laminations; IEC 1212-2 5.5.3
Charpy Impact Unnotched >= 5.00 J/cm²>= 23.8 ft-lb/in²Parallel to laminations; IEC 1212-2 5.5.2
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance >= 1.00e+10 ohm>= 1.00e+10 ohmAfter immersion in water; IEC 1212-2 6.3
Dielectric Constant  <= 5.5
@Frequency 48.0 - 62.0 Hz
<= 5.5
@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
 <= 5.5
@Frequency 1e+6 Hz
<= 5.5
@Frequency 1e+6 Hz
IEC 1212-2 6.2
Dielectric Breakdown >= 35000 V
@Temperature 90.0 °C
>= 35000 V
@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Dissipation Factor  <= 0.040
@Frequency 48.0 - 62.0 Hz
<= 0.040
@Frequency 48.0 - 62.0 Hz
IEC 1212-2 6.2
 <= 0.040
@Frequency 1e+6 Hz
<= 0.040
@Frequency 1e+6 Hz
IEC 1212-2 6.2
Comparative Tracking Index >= 180 V>= 180 VIEC 1212-2 6.4
 
Descriptive Properties
Thermal Endurance155 T.I.IEC 1212-2 7.1
Water Absorption< 34 mgIEC 1212-2 8.2; Test piece 50 x 50 x 10 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Saint-Gobain Chemlam® 3300 High Mechanical Performance Industrial Laminate
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
American Birch Wood
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet

PHIPPE906 / 121910

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.