Materials to create long-lasting, flame retardant products ranging from electronic parts to medical devices, gaming machine components and automotive parts. Inno-FR™ liquid plastic casting resins meet UL 94 V-O requirements. Several of the polyurethanes are Yellow Card certified at Underwriters Laboratories (UL).Information provided by © RAMPF Tooling Solutions GmbH & Co. KG |