MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Momentive Performance Materials GE Silicones SilGlaze II SCS2811-D1 Silicone Backbedding Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: SilGlaze II SCS2811-D1 silicone back bedding sealant is a one-part, neutral, very fast cure, high modulus silicone sealant that develops significant green strength in the early cure hours. SilGlaze II SCS2811-D1 silicone back bedding sealant may be an excellent candidate for use as a bedding seal in the construction of residential and commercial doors and windows. Features: Silicone Durability, Primerless Adhesion, Fast Green Strength, ±25% Movement Capacity, Standard Equipment, Excellent Process ability, Easy Repairs, Product Chemistry.

Applications: SilGlaze II SCS2811-D1 sealant may be used for in-shop window fabrication as a bedding bead or for cap, toe, heel head applications and for general purpose sealing.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatile Organic Compounds (VOC) Content <= 34 g/l<= 34 g/lUncured; WPSTM C1454
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2424ASTM D2240
Tensile Strength, Ultimate 1.95 MPa283 psiASTM D412
Elongation, Ultimate 415 %415 %ASTM D412
Peel Strength 5.96 kN/m
@Temperature 23.9 °C,
Time 1.81e+6 sec
34.0 pli
@Temperature 75.0 °F,
Time 504 hour
50% Relative Humidity.; ASTM C794
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -48.3 °C-55.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 23.0 °C
@Time 1.81e+6 sec
73.4 °F
@Time 504 hour
Cure as Tested at 50% RH
Cure Time 4320 - 5760 min72.0 - 96.0 hourMost common bead sizes.
 <= 1440 min
@Temperature 24.0 °C
<= 24.0 hour
@Temperature 75.2 °F
1/4" deep section.
Tack-Free Time 15.0 min
@Temperature 22.2 °C
0.250 hour
@Temperature 72.0 °F
50% RH; ASTM C679
Working Life 5.00 - 10.0 min5.00 - 10.0 min
 
Descriptive Properties
AppearancePaste
ColorTranslucentSilGlaze II SCS2811-D1 sealant
Consistency / Sag0.1” max.ASTM D2202
Joint Movement Capability+/- 25%ASTM C719.
Silicone Content (%)100Uncured
UV & Weathering ResistanceExcellentGE 20 yr study

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9921 / 265731

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.