MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Hexcel® HexPly® M90 Epoxy Resin Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® M90 is a hot melt, thermosetting, high tack epoxy resin matrix, specifically designed for prepreg applications for which short cure cycles from 100°C and above, and low pressure are required. M90 can be used for the manufacture of a large range of aerospace components, suitable for the cure of thin and thick sections. M90 exhibits a long out-life at ambient conditions.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 - 1.22 g/cc0.0397 - 0.0441 lb/in³
Viscosity  1000 cP
@Temperature 105 °C
1000 cP
@Temperature 221 °F
@2°C/min
 1.00e+6 cP
@Temperature 40.0 °C
1.00e+6 cP
@Temperature 104 °F
@2°C/min
 1.00e+7 cP
@Temperature 130 °C
1.00e+7 cP
@Temperature 266 °F
@2°C/min
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg >= 100 °C>= 212 °FWet (70°C/85%RH to saturation), Onset Log scale; EN 6032
 135 °C275 °FDry, Onset Log scale; EN 6032
 
Processing PropertiesMetricEnglishComments
Cure Time  26.0 - 40.0 min
@Temperature 120 °C
0.433 - 0.667 hour
@Temperature 248 °F
time to 95% conversion; ISO 11357-5
 35.0 - 55.0 min
@Temperature 110 °C
0.583 - 0.917 hour
@Temperature 230 °F
time to 95% conversion; ISO 11357-5
 55.0 - 85.0 min
@Temperature 100 °C
0.917 - 1.42 hour
@Temperature 212 °F
time to 95% conversion; ISO 11357-5
Shelf Life  1.50 Month
@Temperature 23.0 °C
1.50 Month
@Temperature 73.4 °F
Out Life
 6.00 Month
@Temperature 5.00 °C
6.00 Month
@Temperature 41.0 °F
Alternative Shelf Life
 18.0 Month
@Temperature -18.0 °C
18.0 Month
@Temperature -0.400 °F
Shelf Life
 
Descriptive Properties
ColorOff white -Yellowish

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9164 / 322320

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.