MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ASTM A36 Steel, plate
Categories: Metal; Ferrous Metal; ASTM Steel; Carbon Steel; Low Carbon Steel

Material Notes: Steel for general structural purposes including bridges and buildings.

Minimum Cu content when copper steel is specified.

Tests performed in transverse direction for plates wider than 590 mm.

Key Words: UNS K02600
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/ccTypical of ASTM Steel
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 400 - 550 MPa
Tensile Strength, Yield 250 MPa
Elongation at Break 20 %in 200 mm
 23 %In 50 mm.
Modulus of Elasticity 200 GPa
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.26
Shear Modulus 79.3 GPa
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.25 - 0.29 %
Copper, Cu 0.20 %
Iron, Fe 98 %
Manganese, Mn 1.03 %
Phosphorus, P <= 0.040 %
Silicon, Si 0.28 %
Sulfur, S <= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A36 Steel, bar
ASTM A572 Steel, grade 50
ASTM A36 Steel, flange
AISI 1018 Steel, cold drawn
ASTM A500 Steel, grade B, shaped structural tubing

MSA36C / 14017

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.