MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Total PSI 945 Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Polystyrene 945 is designed for injection molding applications requiring superior toughness. This polymer is a high impact polystyrene with excellent gloss and falling dart properties. The impact and gloss levels achievable with 945 allow design engineers to use this polymer instead of more expensive engineering polymers.

Applications such as industrial guards, appliance housings, toys, and industrial spools are candidates for 946.

Information provided by Total Petrochemicals, Inc.

Key Words: Super high impact, toughness
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 19.3 MPa2800 psiASTM D638
Elongation at Yield 55 %55 %ASTM D638
Tensile Modulus 1.86 GPa270 ksiASTM D638
Flexural Strength 38.6 MPa5600 psiASTM D790
Flexural Modulus 2.14 GPa310 ksiASTM D790
Izod Impact, Notched 1.39 J/cm2.60 ft-lb/inASTM D256
Falling Dart Impact 15.82 J11.67 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 90.0 °C194 °FHeat Distortion, Annealed; ASTM D648
Vicat Softening Point 95.6 °C204 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 60 %60 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PSC 1540(AS) Crystal Polystyrene
Total PSC 1540(EU) Crystal Polystyrene
Total PSC 525 Polystyrene
Total PSC 523 Polystyrene
A. Schulman CP814-01 Linear, Low-Density Polyethylene

PFIM920 / 38325

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.