MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals INCOLOY® 27-7MO Super-Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: INCOLOY® alloy 27-7MO (UNS S31277; EP 1,263,999 B1) is an advanced 7% molybdenum super-austenitic stainless steel offering corrosion resistance in most environments superior to 6% molybdenum super-austenitic stainless steels. In many environments, alloy 27-7MO offers resistance approaching that of much more highly alloyed materials such as INCONEL alloys 625, 22, and C-276.

Applications for INCOLOY alloy 27-7MO are found in the pollution control, power, marine, chemical processing, pulp and paper, and oil and gas industries. The alloy offers a unique combination of corrosion resistance, high strength and ease of fabrication.

Information Provided by Special Metals Corporation

Key Words: UNS S31277; ASTM A 182, A 213, A 240, A 249, A 312, A 479
ASME SA 182, SA 213, SA 240 SA 249, SA 312, SA 479; ASME Code Case 2458
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.02 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 95Annealed
Hardness, Vickers 2250% cold work
 38050% cold work
Tensile Strength, Ultimate 120000 psiAnnealed
Tensile Strength, Yield 414 MPa
@Strain 0.2 %
Annealed
Elongation at Break 50 %
Modulus of Elasticity 138 GPa
@Temperature 816 °C
 153 GPa
@Temperature 649 °C
 164 GPa
@Temperature 482 °C
 174 GPa
@Temperature 316 °C
 184 GPa
@Temperature 149 °C
 191 GPa
@Temperature 22.0 °C
Poissons Ratio 0.29
@Temperature 22.0 °C
 0.30
@Temperature 149 °C
 0.30
@Temperature 316 °C
 0.31
@Temperature 816 °C
 0.32
@Temperature 482 °C
 0.33
@Temperature 649 °C
Shear Modulus 53.0 GPa
@Temperature 816 °C
 57.0 GPa
@Temperature 649 °C
 62.0 GPa
@Temperature 482 °C
 67.0 GPa
@Temperature 316 °C
 71.0 GPa
@Temperature 149 °C
 74.0 GPa
@Temperature 22.0 °C
Shear Strength 10.8 ksiAnnealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 604 ohm-cir-mil/ft
Magnetic Permeability 1.004
@Temperature 23.0 °C
 <= 1.01
@Temperature -30.0 °C
200 Oersted (15.9 kA/m); Annealed
 <= 1.01
@Temperature -30.0 °C
200 Oersted (15.9 kA/m); 50% Cold Worked
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.21 µm/m-°C
@Temperature -190 °C
Mill Annealed Condition
 13.93 µm/m-°C
@Temperature -50.0 °C
Mill Annealed Condition
 15.46 µm/m-°C
@Temperature 200 °C
Mill Annealed Condition
 15.85 µm/m-°C
@Temperature 350 °C
Mill Annealed Condition
 16.19 µm/m-°C
@Temperature 500 °C
Mill Annealed Condition
 16.86 µm/m-°C
@Temperature 650 °C
Mill Annealed Condition
Specific Heat Capacity 0.454 J/g-°C
Thermal Conductivity 10.114 W/m-K
@Temperature 23.0 °C
 12.126 W/m-K
@Temperature 100 °C
 16.295 W/m-K
@Temperature 300 °C
 20.039 W/m-K
@Temperature 500 °C
 24.069 W/m-K
@Temperature 700 °C
 25.852 W/m-K
@Temperature 900 °C
 28.947 W/m-K
@Temperature 1100 °C
Melting Point 1350 - 1390 °C
Solidus 1350 °C
Liquidus 1390 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Chromium, Cr 20.5 - 23 %
Copper, Cu 0.50 - 1.5 %
Iron, Fe 35.54 - 46.2 %Balance
Manganese, Mn <= 3.0 %
Molybdenum, Mo 6.5 - 8.0 %
Nickel, Ni 26 - 28 %
Nitrogen, N 0.30 - 0.40 %
Phosphorus, P <= 0.030 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.010 %
 
Descriptive Properties
Critical Crevice Temperature (°C)45ASTM G48 Test Methods C and D
 60in "Green Death" solution
Critical Pitting Temperature (°C)>85ASTM G48 Test Methods C and D
 75in "Green Death" solution
Pitting Resistance Equivalent Number43

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek MTEK 29-10 Cast UNS J93403 Heat Resistant Stainless Steel
Special Metals INCOLOY® 25-6HN Super-Austenitic Stainless Steel
ATI Allvac® XM-19™ / ATI 50™ UNS S20910 Specialty Steel
Special Metals INCOLOY® A-286 Iron-Nickel-Chromium Alloy (UNS S66286)
3M Nextel™ 312 Industrial Ceramic Fiber

NINDA14 / 98905

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.