MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Arkema Rilsan® BESNO MED Nylon 11
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Unreinforced

Material Notes: Rilsan® PA 11 BESNO MED is a polyamide produced from a renewable source. This grade dedicated to extrusion offers the highest quality and it is specially designed to meet the stringent requirements of the medical applications such as minimally invasive devices. Upon request letters regarding USP Class VI testing can be provided. Designation: PA11, E, 22-010

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
 1.02 g/ccCond.; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 71
@Time 15.0 sec
Dry; ISO 7619-1
Tensile Strength, Yield 40.0 MPaCond.; ISO 527-1/-2
Elongation at Break >= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 6.0 %Cond.; ISO 527-1/-2
Tensile Modulus 1200 MPaCond.; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²
@Temperature -30.0 °C
Cond.; ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
Cond.; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 186 °C10°C/min; Dry; ISO 11357-1/-3
 
Descriptive Properties
%Bio-Based100ASTM D6866
Bio-BasedYes
Form as DeliveredPellets
Moisture SensitiveYes
Processing MethodsOther Extrusion
 Profile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsamid® AESNO MED Nylon 12
Arkema Rilsan® BESNO P40 TL PA11
Arkema Rilsan® BESNO TL PA11
Arkema Rilsan® BESNO P20 TL PA11
Arkema Rilsan® BESNO 23 TL4CC PA11

PARKG675b / 142949

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.