MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Master Bond UV22DC80TK One component, nanosilica filled, dual cure system with UV and heat curing mechanisms
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Thixotropic moderate viscosity
  • Minimal shrinkage upon curing
  • Low coefficient of expansion
  • Cures in shadowed out areas at 80°C
Master Bond UV22DC80TK is a nanosilica filled, UV dual cure system. The secondary cure is accomplished by adding heat, with the minimum temperature being 80°C. Essentially, this epoxy based system will cure readily upon exposure to UV light and if there are any shadowed out areas, heating at 80°C will complete the cure. The 80°C curing feature is particularly useful given the sensitivity of many plastics to elevated temperatures. The consistency of UV22DC80TK can best be described as thixotropic, moderate viscosity. It dispenses readily, but it is not as free flowing as lower viscosity versions. This UV is a cationic type cure and is not oxygen inhibited. It bonds well to a wide variety of substrates including metals, glass, ceramics and most plastics. UV22DC80TK has very good chemical resistance to many acids, bases, fuels and solvents. It is a superb electrical insulator, also it is able to withstand rigorous thermal cycling. The service temperature range is -60°F to +350°F. As a nanosilica filled system, it has exceptionally low shrinkage upon curing and stellar dimensionally stability. Typically the UV portion occurs in 10-30 seconds at 365 nm with 10-40 milliwatts/cm2 of output. Areas not cured because of shadowing effects can be readily cured at 80°C for 30-60 minutes. Post curing at 125-150°C for 15-30 minutes will increase the Tg. In addition to bonding, his UV can be used for small encapsulations as it will cure in thickness up to 0.075 inches. The combination of special flow properties and dual curing is especially intriguing. This epoxy is a viable option for high tech aerospace, electronics, optical and specialty OEM applications.

Product Advantages:

  • One component system; no mixing needed
  • Dual curing mechanism allows for curing in shadowed out areas and rapid fixturing time at 80°C
  • No oxygen inhibition
  • Very low shrinkage upon curing
  • Nano filled, high dimensional stability
  • NASA low outgassing

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Water Absorption <= 1.0 %<= 1.0 %3 month immersion, 75°F
Viscosity 40000 - 80000 cP40000 - 80000 cP
Linear Mold Shrinkage <= 0.010 cm/cm<= 0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75 - 8575 - 85
Tensile Strength 41.4 - 55.2 MPa6000 - 8000 psi
Tensile Modulus 2.76 - 3.10 GPa400 - 450 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 4.1
@Frequency 60 Hz
4.1
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 - 35.0 µm/m-°C16.7 - 19.4 µin/in-°F
Maximum Service Temperature, Air 177 °C351 °F
Minimum Service Temperature, Air -51.0 °C-59.8 °F
Glass Transition Temp, Tg 130 - 135 °C266 - 275 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.521.52
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 4.44 - 10.0 °C
6.00 Month
@Temperature 40.0 - 50.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM624 / 249020

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.