MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M CP 25WB+ Fire Barrier Sealant
Categories: Polymer; Thermoset

Material Notes: 3M Fire Barrier Sealant CP 25WB+ is a high-performance, ready-to-use, gun-grade, latex-based, intumescent sealant that dries to form a monolithic fire-stop seal that also acts as a barrier to airborne sound transmission. 3M Fire Barrier Sealant CP 25WB+ helps control the spread of fire, smoke and noxious gasses before, during and after exposure to a fire when installed in accordance with a listed through penetration or fire-resistive joint assembly system. 3M Fire Barrier Sealant CP25WB+ firestops blank openings and penetrations passing through fire-rated floor, floor/ceiling or wall assemblies and other fire-rated interior building construction. The unique intumescent property of this material allows 3M Fire Barrier Sealant CP25WB+ to expand and help maintain a firestop penetration seal for up to 4 hrs as penetratants are exposed to fire. 3M Fire Barrier Sealant CP25WB+ exhibits excellent adhesion to a full range of construction substrates and penetrants. No mixing is required.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatile Organic Compounds (VOC) Content >= 1.0 g/l>= 1.0 g/lVOC Less H2O and Exempt Solvents
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545ASTM D2240
Tensile Strength at Break 0.590 MPa85.6 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.0 °C180 °F
Minimum Service Temperature, Air -28.0 °C-18.4 °F
Shrinkage 28 %28 %Volume; ASTM C1241
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 4.00 °C>= 39.2 °FApplication; ASTM C1299
 <= 50.0 °C<= 122 °FApplication; ASTM C1299
Cure Time 30.0 - 60.0 min0.500 - 1.00 hourDry to touch, RT @ 50%RH
Tack-Free Time 10.0 min0.167 hourRT @ 50% RH
Shelf Life >= 2.00 Month>= 2.00 Month
 
Descriptive Properties
AppearanceRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35439 / 170186

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.