MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Advanced Petrochem PP 1104 K Propylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Description: Advanced-PP 1104 K is a propylene homopolymer with medium molecular weight distribution (MWD) and narrow MFR range. Main application is OPP core layers and high performance weaving tapes. eg for carpet backing. The product is free from metal stearates and functional additives like slip agents and is therefore in particular suitable for metallisable BOPP film and provides low water-carry over.

Application: OPP films ( stenter frame process), weaving tapes.

Regulatory Information: The Grade Advanced-PP 1104K and additives incorporated comply with United States FDA Regulation 21CFR 177.1520 Olefin Polymers and European Regulation (EU) 10/2011 (and its amendments). Specific information is available upon request.

Information provided by Advanced Petrochemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ISO 1183
Melt Flow 3.2 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.2 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 74.0 MPa10700 psiH 358/30; ISO 2039-1
Tensile Strength, Yield 34.0 MPa4930 psi50 mm/min; ISO 527-2
Elongation at Break >= 50 %>= 50 %50 mm/min; ISO 527-2
Elongation at Yield 9.0 %9.0 %50 mm/min; ISO 527-2
Modulus of Elasticity 1.45 GPa210 ksi1 mm/min; ISO 527-2
Charpy Impact Unnotched 19.0 J/cm²90.4 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 163 °C325 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FISO 75-2
Vicat Softening Point 154 °C
@Load 1.02 kg
309 °F
@Load 2.25 lb
A50; ISO 306
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAVPC006 / 249454

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.