MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Qualchem Danamid AFGF-50 Polyamide 66, 50% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Reinforced with glass fiber

Information provided by Qualchem Zrt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³DIN 53479
Filler Content 48 - 52 %48 - 52 %
Moisture Absorption at Equilibrium 1.2 - 1.6 %1.2 - 1.6 %DIN 53714
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 180 MPa>= 26100 psi50 mm/min; ISO 527-1,2
Elongation at Break 3.0 %3.0 %ISO 527-1,2
Tensile Modulus >= 9.50 GPa>= 1380 ksiISO 527-1,2
Charpy Impact Unnotched >= 3.00 J/cm²
@Temperature 23.0 °C
>= 14.3 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
Charpy Impact, Notched  >= 0.800 J/cm²
@Temperature -20.0 °C
>= 3.81 ft-lb/in²
@Temperature -4.00 °F
DIN 53453
 >= 1.00 J/cm²
@Temperature 23.0 °C
>= 4.76 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDIN 53482
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FDIN 53461
Flammability, UL94 HB
@Thickness 4.00 mm
HB
@Thickness 0.157 in
MSZ 10383

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Radici Radilon® A RCF3505 (dry) Nylon 66
Radici Radilon® A RCF3505 (cond.) Nylon 66
Radici Radilon® A CF350 (cond.) Nylon 66
Celanese Zytel® HTNFG52G35HSL BK011 PA6T/66-GF35
Celanese Zytel® FG101L NC010 PA66

PQUALC07 / 58419

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.