MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lushan DP-1 Polypropylene sintered powder, Ultra Fast Cure
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: PP sintered powder Lushan DP-1 is used on anti-corrosion coated steel pipe Polypropylene top coats and applied in oil & gas submarine counterweight pipeline to make a non-slid surface to avoid skidding. PP sintered powder Lushan DP-1 is combined with more than 10 years practice and experience on the area of oil & gas pipeline anti-corrosion. PP sintered powder Lushan DP-1 has good stability, wide processing technology, strong adhesion with the outer PP layer, high mechanical strength and ageing resistance property, etc.

Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³GB/T1033.1
Particle Size 200 - 500 µm200 - 500 µmGB/T 12005.7
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 22.0 MPa3190 psiGB/T1040.1
Flexural Modulus 0.600 GPa87.0 ksiGB/T94341
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.050 %0.050 %HG/T2751

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUSH008 / 150006

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.