MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Proteus™ Homopolymer PP Natural Natural Homo-Polymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: These polypropylene shapes exhibit a high strength-to-weight ratio, excellent chemical and corrosion resistance capabilities, thermoformability, and zero moisture absorption. Additionally, this grade of polypropylene is also FDA and NSF compliant, making it ideal for chemical processing, food processing, storage, and medical applications.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78.0ISO 868
Tensile Strength 34.0 MPaISO 527-1/-2 (7)
Elongation at Yield 6.00 %ISO 527-1/-2 (7)
Compressive Yield Strength 15.0 MPa
@Strain 1.00 %
ISO 604 (10)
 26.0 MPa
@Strain 2.00 %
ISO 604 (10)
 43.0 MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 12.0 kJ/m²Double Notched
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Strength 570 kV/inASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 43.0 µin/in-°FASTM E-831 (TMA)
 150 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.220 W/m-K
Melting Point 327 °FASTM D3418
Maximum Service Temperature, Air 190 °FContinuous Use Temperature in Air after 20000 hr
 
Compliance PropertiesOriginal ValueComments
FDA Yes
NSF Yes
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Acceptable
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Semitron™ CMP LL5 PET Polyester
Mitsubishi Chemical Advanced Materials Semitron™ CMP XL20 PAI
Mitsubishi Chemical Advanced Materials Semitron™ ESd 225 POM Extruded, Static Dissipative Acetal
Mitsubishi Chemical Advanced Materials Semitron™ ESd 410C PEI Static Dissipative Polyetherimide
Mitsubishi Chemical Advanced Materials Semitron™ ESd 420 PEI Static Dissipative Polyetherimide

P1SMP66cc / 221026

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.