MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
MarkeTech Dermagrain 1200 Microcrystalline Alumina for Microdermabrasion  (discontinued **)
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Used for microdermabrasion. Dermagrain is a specially graded high purity micro crystalline aluminum oxide made from Bayer process alumina which results in final product purity of 99.55%. It has been fused at nearly 4000°F to make an extremely stable material with the identical crystal structure of sapphire. Aluminum oxide is completely inert and pH neutral. Components made from aluminum oxide are approved for use by the FDA as prosthetic and dental implants.

After fusion the material is processed to form grains with blocky, sharp edges to enhance abrasive properties. It is then graded into a tightly controlled particle size distribution. Close examination under a microscope will show that the individual particles are clear grains of sapphire and will sparkle like diamond under reflected light. Because they are clear and absorb light, the grains appear slightly off white in color. Dermagrain 1200 has a D50 (median) particle diameter of 100 microns.

Data provided by the supplier, MarkeTech International.

MarkeTech International is no longer in business.

Key Words: Al2O3; Corundum
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.95 g/cc
Apparent Bulk Density 1.64 - 1.72 g/cc
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 2000Knoop 100 Hardness
Hardness, Mohs 9.0
 
Thermal PropertiesOriginal ValueComments
Melting Point 2022 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 99.55 %
Alkalis 0.30 %
CaO 0.030 %
Fe2O3 0.040 %
MgO 0.020 %
SiO2 0.050 %
TiO2 0.010 %
 
Descriptive Properties
ColorOff White

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6082-T4
Mitsubishi Chemical Advanced Materials Semitron™ ESd 420 V PEI
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Morgan Advanced Ceramics HIP Vitox™ Bio-compatible Alumina
1200 Aluminum Composition Spec

C5MT75 / 371

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.