MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Momentive Performance Materials GE Sealants & Adhesives Painter’s Siliconized Acrylic Latex Caulk
Categories: Polymer; Thermoset; Silicone

Material Notes: Painter’s Siliconized Acrylic Latex is an all-purpose paintable caulk ideal for interior and exterior paint preparation. Painter’s caulk is low in odor, guns out effortlessly, tools smoothly and cleans-up easily with soap and water. This formulation resists cracking and offers good durability and flexibility. The fully cured caulk is resistant to stain-causing mold and mildew growth. Painter’s caulk creates a seal that is long-lasting for professional results.

Features: Backed by a limited 40-year durability guarantee, Paint-Friendly, Durable Adhesion and flexibility for long lasting results, Cured caulk forms a water resistant seal, Low odor and low VOC (Meets CARB VOC Limits), Easy application, Soap and water clean-up.

Applications: Painter’s Siliconized Acrylic Latex caulk can be used in a wide variety of interior and exterior applications, including trim, crown molding, baseboards, vents and around doors, windows.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.65 g/cc0.0596 lb/in³Uncured
Solids Content 79 - 83 %79 - 83 %By weight. Uncured.; ASTM C1250
Volatile Organic Compounds (VOC) Content <= 37 g/l<= 37 g/lUncured. Excluding water & exempt compounds
 
Processing PropertiesMetricEnglishComments
Processing Temperature 40.0 - 100 °C104 - 212 °FApplication Temp
Cure Time 1440 min24.0 hour3/16 inch bead size
Tack-Free Time 45.0 min0.750 hourASTM C679
 
Descriptive Properties
AppearanceSmooth & CreamyUncured
BaseAcrylic Latex
Carb Chem Curing VOC<1.5 wt.%
ColorWhiteMAP110WT 12C
Consistency / SagPassedUncured. ASTM C693
Freeze/Thaw StabilityPassed / 5 Cycles at 0°FUncured. ASTM C731.
OdorSlight AcrylicUncured
Paint Ready Time45 minutes
Water Ready24 hoursUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9947 / 265758

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.