MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

DSM Somos® 7120 Epoxy Photopolymer, UV & Thermal Postcure  (discontinued **)
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset; Epoxy

Material Notes: Description

DSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, undistorted thin walls and down-facing surfaces and exhibits good processing latitude.

Application

Somos® 7120 Photopolymer is used in the solid imaging process to build three-dimensional parts.

Information Provided by DSM Desotech Inc.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. Industry leaders in providing high quality Rapid Prototyping and Additive Manufacturing solutions using all major 3D printing systems including SLA Rapid Prototypes. Fast and Free online quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc
@Temperature 25.0 °C
0.0408 lb/in³
@Temperature 77.0 °F
Viscosity 700 cP
@Temperature 30.0 °C
700 cP
@Temperature 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888ASTM D2240
Tensile Strength, Yield 63.0 MPa9140 psiASTM D638M
Elongation at Break 2.3 - 4.1 %2.3 - 4.1 %ASTM D638M
Modulus of Elasticity 2.588 GPa375.4 ksiASTM D638M
Flexural Strength 113 MPa16400 psiASTM D790M
Flexural Modulus 2.877 GPa417.3 ksiASTM D790M
Izod Impact, Notched 0.320 J/cm0.599 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) <= 97.0 °C<= 207 °FASTM D648
 
Descriptive Properties
AppearanceTransparent Amber
Dp (mm)0.123Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2)64Exposure that gives 0.254mm thickness
E5 (mJ/cm2)23Exposure that gives 0.127mm thickness
Ec (mJ/cm2)8Critical exposure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 823 RTM Liquid Epoxy Resin
Master Bond EP46HT-2ND2 Two Part Epoxy
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting
Hexcel® HexPly® F185 Epoxy Resin

PDSMT037 / 93557

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.