MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Total Lacqtene® 2007 TN 61 HDPE pipe  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: LACQTENE® 2007 TN 61 is a high density homopolymer polyethylene produced by the gas phase polymerization process.

LACQTENE® 2007 TN 61 is best processed between 190 and 230°C.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.961 g/cc0.0347 lb/in³ISO 1183
Melt Flow  0.70 g/10 min
@Load 2.16 kg
0.70 g/10 min
@Load 4.76 lb
ISO 1133
 2.8 g/10 min
@Load 5.00 kg
2.8 g/10 min
@Load 11.0 lb
ISO 1133
High Load Melt Index 47 g/10 min
@Load 21.6 kg
47 g/10 min
@Load 47.6 lb
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666ISO 868
Tensile Strength, Yield 29.0 MPa4210 psiISO 527-2
Elongation at Break >= 700 %>= 700 %ISO 527-2
Flexural Modulus 1.55 GPa225 ksiISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 136 °C277 °FISO 3146
Vicat Softening Point 132 °C270 °FISO 306
 
Descriptive Properties
Food StatusConforms to both European and American Food contact regulations.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos K38-20-138 Pipe Extrusion Grade Polyethylene
Formosa Plastics Formolene® HP4306 Pipe HDPE
LyondellBasell Hostalen CRP 100 S YELLOW High Density Polyethylene (HDPE), Pipe Grade
Kazanorgsintez PE2NT 11-9 High Density Polyethylene Composite
Kazanorgsintez PE2NT 11-285D High Density Polyethylene Composite

PFINAP142 / 38725

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.