MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik ACEMATT® TS 100 Silica
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Properties and applications: ACEMATT TS 100 is an untreated thermal silica characterized by very high matting efficiency combined with very high transparency. Thanks to the unique properties, ACEMATT TS 100 is particularly suitable for coating systems that are difficult to matt. It can be used in water-based coatings, waterborne UV coatings, clear coatings, coatings for leather and films, as well as all types of top coats. Coating formulations containing ACEMATT TS 100 show outstanding resistance against household chemicals. Due to the high purity and extremely low electrical conductivity, ACEMATT TS 100 is outstanding for applications in sensitive coating systems such as solder resist. ACEMATT TS 100 improves flow behavior and increases storage stability in powder coatings.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 9.5 µm9.5 µmd50; ISO 13320-1
pH 6.56.55% in water; ISO 787-9
Specific Surface Area 250 m²/g250 m²/gISO 9277
 
Component Elements PropertiesMetricEnglishComments
SiO2 >= 99 %>= 99 %ISO 3262-19

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cookson Group Plaskon® 150.401 Encapsulation Resin

PEVONIM030 / 197234

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.