Product Description: Foral™ 85-E Ester of Hydrogenated Rosin is a very pale, thermoplastic ester resin derived from glycerol and a highly stabilized rosin that has outstanding resistance to oxidation, and to discoloration caused by heat and aging. Foral™ 85-E Ester of Hydrogenated Rosin can be used as a tackifier resin in various types of adhesives, and in protective and barrier-type coatings that require a high degree of color retention and oxidation resistance. Application/Uses: - Caulks and Sealants
- Contact Adhesives
- Hot Melt Adhesives
- Laminating
- Nonwovens
- Packaging
- Pressure sensitive adhesives
- Rubber and Plastic Modification
- Solventborne Adhesives
- Tapes and Labels
- Wax Modification
Key Attributes:- Excellent resistance to oxidation and discoloration
- Exceptional cutaneous tolerance
- Light color
- Low odor
- Medium softening point
- Thermoplastic hydrogenated resin
- Wide solubility and compatibility range
Information provided by Eastman |