MG9641B is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of articles which require good rigidity, good flow properties and high impact strength. Applications: crates, and snow pulcas.Information provided by Borealis AG |