MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Interior application for thick & thin gauge profile application.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.39 g/ccASTM D1638
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81ASTM D2240
Tensile Strength, Yield 45.9 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2680 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 84.1 MPaASTM D790
Flexural Modulus 2880 MPaASTM D790
Izod Impact, Unnotched 70.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Compression Molded; ASTM D256
Dart Drop Total Energy 53.8 J/cm
@Temperature 23.0 °C
Procedure A, C.125; ASTM D4226
 102 J/cm
@Temperature 23.0 °C
Procedure B, C.125; ASTM D4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 67.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Flammability, UL94 V-0UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 191 - 204 °C
 
Descriptive Properties
FeaturesLow Gloss
 Medium Impact Resistance
FormsPowder
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
 Profile Extrusion
PVC Cell Classification12344ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Interior Parts
 Profiles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Dry Blend E7009 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Fittings 87431 PVC, Rigid
Geon® Performance Solutions Vinyl Fittings 210(HR) Polyvinyl Chloride, Rigid
Geon® Performance Solutions 85890 Molding PVC
Axiall 5009 Rigid PVC, Molding

PH0POL0549 / 145118

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.