MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik 11R51 HV Spring wire
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Sandvik 11R51 HV is a vacuum remelted austenitic stainless steel alloyed with molybdenum. The grade is characterized by high tensile strength and high resistance to corrosion, fatigue and relaxation. Vacuum remelted Sandvik 11R51 HV offers higher cleanliness compared to Sandvik 11R51, which if usually required for applications within, for example, the medical area. Compared to most other steels of ASTM 302 type (for example Sandvik 12R10/gusab T302), Sandvik 11R51 HV offers:
  • Higher tensile strength and tempering effect
  • Higher relaxation resistance, especially at elevated temperatures
  • Higher fatigue strength
  • Better corrosion resistance, through the addition of molybdenum
Service temperature: -200 to 300°C (330 to 570°F).

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 300 °C572 °F
Minimum Service Temperature, Air -200 °C-328 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.080 %0.080 %
Chromium, Cr 17 %17 %
Manganese, Mn 1.7 %1.7 %
Molybdenum, Mo 0.70 %0.70 %
Nickel, Ni 7.5 %7.5 %
Phosphorus, P <= 0.025 %<= 0.025 %
Silicon, Si 1.5 %1.5 %
Sulfur, S <= 0.020 %<= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik 11R51 Spring Wire
Sandvik 75X1 Spring Wire
Sandvik 5R60/5R62 Spring Wire
Sandvik 5R10 Spring wire
Sandvik 12R10L Spring wire

NSANDV5062 / 199626

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.