Dexflex thermoplastic polyolefins (TPOs) are in use in applications once reserved for more expensive engineering resins. The performance of these TPOs, combined with their quality and consistency, makes them cost-effective alternatives in automotive applications. Dexflex 711 BLK is a thermoplastic olefin elastomeric (TPO) compounded with postindustrial/ post-consumer recycled materials. It is typically used for use in applications that are black but not color-matched, and that require very good processing characteristics. Applications: Exterior Automotive Applications, Underhood Information provided by LyondellBasell. |