MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shin-Etsu Silicones KE-167U Low Temperature Silicone Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: ShinEtsu KE167U is a phenyl (PVMQ) silicone compound. This product is designed for good low temperature characteristics.

Product Features:

  • A broad range of service temperatures from 100 to +260°C (148 to +500°F.)
Typical Applications:
  • Leisure underwater glasses.
  • Leisure underwater goggles.
  • Low temperature gaskets

Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555
Tensile Strength at Break 12.26 MPa1778 psi
Elongation at Break 550 %550 %
Tear Strength 35.1 kN/m200 pliDie B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -100 °C-148 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 240 min
@Temperature 200 °C
4.00 hour
@Temperature 392 °F
Post
 
Descriptive Properties
Cure TypePost Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shin-Etsu Silicones C-19A Silicone Gum
Shin-Etsu Silicones FEA-261U Fluorosilicone Elastomer
Shin-Etsu Silicones KE-109A/B Silicone, Potting/Encapsulation RTV
Shin-Etsu Silicones KE-1843 Silicone, RTV Adhesive/Sealant
Shin-Etsu Silicones KE-3421 Silicone, RTV Conformal Coating

PSHIN216 / 177727

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.