MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

MOL Group TIPELIN 7000F HDPE, Blown Film
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade; High Density Polyethylene (HDPE), Film Grade

Material Notes: Description: TIPELIN 7000F is a high density bimodal polyethylene copolymer (with butene-1 as comonomer) intended for blown film of products with excellent mechanical strength and good stiffness. It offers good processability at high speed. The grade contains antioxidant and acid scavenger.

Applications: TIPELIN 7000F is recommended for disposal waste bags, grocery bags and ultra-thin films. Recommended film thickness is 0.006 to 0.06 mm.

(1) Average mechanical property values of several measurements carried out on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291). (2) Average mechanical property values of several measurements on film (MD = machine direction, TD = trans direction) thickness of 0.015 mm, blow up ratio 4:1.

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.955 g/cc0.0345 lb/in³1; ISO 1183-1
Oxidative Induction Time (OIT) 50 min
@Temperature 200 °C
50 min
@Temperature 392 °F
EN 728
Melt Flow  0.080 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.080 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 0.30 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.30 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 9.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
9.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 64641; ISO 868
Film Tensile Strength at Yield, MD 27.0 MPa3920 psi2; ISO 527-3
Film Tensile Strength at Yield, TD 24.0 MPa3480 psi2; ISO 527-3
Film Elongation at Break, MD 500 %500 %2; ISO 527-3
Film Elongation at Break, TD 550 %550 %2; ISO 527-3
Flexural Modulus 1.50 GPa218 ksi1; ISO 178
Izod Impact, Notched (ISO) 16.0 kJ/m²7.61 ft-lb/in²1; ISO 180/A
Impact 85852, Spencer; ASTM D 3420
Elmendorf Tear Strength MD 15 g15 g2; ISO 6383-2
Elmendorf Tear Strength TD 175 g175 g2; ISO 6383-2
Dart Drop Test 185 g0.408 lb2; ISO 7765-1 method A
Film Tensile Strength at Break, MD 67.0 MPa9720 psi2; ISO 527-3
Film Tensile Strength at Break, TD 45.0 MPa6530 psi2; ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 129 °C264 °F1; ISO 306/A 120
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 220 °C356 - 428 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOLG022 / 297188

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.