MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV 4775B42 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 4700 Series are very high flow injection molding engineering grades with excellent UV resistance, elasticity, and surface aesthetics designed for demanding automotive applications including window encapsulation and exterior parts. This product is a black, medium hardness, low density thermoplastic vulcanizate suited for injection molding applications that require superior flow properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: UV Stabilizer

Features: Chemical Resistant; Good Flexibility; Good Processability; High Flow; Low Density; Low Specific Gravity; Medium Hardness; Resilient; UV Resistant; Weather Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Window Encapsulation; Rubber Replacement

RoHS Compliance: RoHS Compliant

Automotive Specifications: BMW Unspecified Color: Black; DAILMLER DBL 5422 Color: Black; DAIMLER DBL 5562.30 Color: Black; FORD WSS-M9P-10A Color: Black; GM QK 3223 L Color: Black; HONDA 73512-T6L Color: Black; PSA Peugeot-Citroen B62 0300 version G Color: Black; RENAULT 32 06 41 D Color: Black; TOYOTA TSM 1707G-7 Color: Black; VAG VW501 23 Color: Black; VAG VW-TL 52381-C Color: Black; VOLKSWAGEN VW 50180 Color: Black

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ISO 1183
Viscosity 200 cP
@Shear Rate 206 1/s,
Temperature 200 °C
200 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  74
@Time 5.00 sec
74
@Time 0.00139 hour
Extruded; ASTM D2240
 76
@Time 5.00 sec
76
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 5.80 MPa841 psiFlow; ASTM D412
 6.30 MPa914 psiAcross Flow; ASTM D412
 5.10 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
740 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 5.17 MPa
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
749 psi
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  3.20 MPa
@Strain 100 %
464 psi
@Strain 100 %
Across Flow; ISO 37
 3.40 MPa
@Strain 100 %
493 psi
@Strain 100 %
Flow; ISO 37
 3.26 MPa
@Strain 100 %,
Treatment Temp. 150 °C
473 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
 3.30 MPa
@Strain 100 %,
Treatment Temp. 135 °C
478 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
Elongation at Break 410 %410 %Flow; ASTM D412
 470 %470 %Across Flow; ASTM D412
 338 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
338 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
 357 %
@Treatment Temp. 150 °C,
Time 605000 sec
357 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tear Strength 31.6 kN/m180 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  24 %
@Temperature 22.8 °C,
Time 79200 sec
24 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 39 %
@Temperature 70.0 °C,
Time 79200 sec
39 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 56 %
@Temperature 125 °C,
Time 252000 sec
56 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 185 - 210 °C365 - 410 °F
Rear Barrel Temperature 180 - 205 °C356 - 401 °F
Middle Barrel Temperature 180 - 205 °C356 - 401 °F
Front Barrel Temperature 180 - 205 °C356 - 401 °F
Nozzle Temperature 185 - 210 °C365 - 410 °F
Mold Temperature 10.0 - 55.0 °C50.0 - 131 °F
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1165 / 237656

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.