MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled
Categories: Ceramic; Other Engineering Material; Ceramic/Metallic Coating; Polymer; Thermoset; Silicone

Material Notes: Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C).

Key Words: High Temperature Coatings
Vendors: Aremco’s HiE-Coat line of high emissivity coatings are black-body systems formulated to significantly improve the thermal efficient of infrared heaters, heat exchangers and furnaces for applications to 2500°F (1371°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/cc
Solids Content 42.5 %by volume
 57.1 %by weight
Volatile Organic Compounds (VOC) Content 637 g/l
Viscosity 250 - 500 cP
Thickness 1.00 milrecommended dry film thickness
 2.40 milwet film thickness
Storage Temperature 40.0 - 90.0 °F
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1100 °F
Flash Point 118 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 120 °FApplication Temperature
Cure Time >= 1.00 hourAir Set prior to curing
 0.750 hour
@Temperature 249 °C
Shelf Life 6.00 Month
 
Descriptive Properties
ColorJet Black
Dry Film Coverage ft2/gal681at 1 mil
ThinnerPM Acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco HiE-Coat™ 840-CM High Emissivity Coating, Inorganic-Ceramic Filled
Aremco HiE-Coat™ 840-M High Emissivity Coating, Inorganic-Ceramic Filled
Gold, Au
Incoloy 840 Superalloy
Emerald Performance Materials HyPox™ RA 840 Bisphenol A Modified Epoxy Resin

PAREM42c / 160512

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.