MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kazanorgsintez Monoethanolamine
Categories: Fluid; Solvent

Material Notes: Production Method: Interaction of ammonia or its water solution with ethylene oxide.

Application: Used in the gas and petroleum industry for absorption of acid gases and sulfur-containing organic compounds, monoethanolamine of the highest and the first class quality is implemented in pharmaceutics, the textile industry, and the carnish-and-liquer industry as well as in the production process or plastics.

Information Provided by Kazanorgsintez

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.015 - 1.018 g/cc
@Temperature 20.0 °C
0.03667 - 0.03678 lb/in³
@Temperature 68.0 °F
Highest Class, First Class
 1.015 - 1.025 g/cc
@Temperature 20.0 °C
0.03667 - 0.03703 lb/in³
@Temperature 68.0 °F
Second Class
 1.015 - 1.05 g/cc
@Temperature 20.0 °C
0.03667 - 0.0379 lb/in³
@Temperature 68.0 °F
Third Class
 
Component Elements PropertiesMetricEnglishComments
Free Water <= 0.60 %<= 0.60 %Highest Class
 <= 1.0 %<= 1.0 %First Class
 <= 3.0 %<= 3.0 %Second Class
 
Descriptive Properties
Color50Hazen units
Mass Content (%)0.6Mass content of diethanolamine, Highest Class
 1Mass content of diethanolamine, 1st Class
 2Mass content of diethanolamine, 2nd Class
 7Mass content of diethanolamine, 3rd Class
 78.8Mass content of monoethanolamine, 3rd Class
 95Mass content of monoethanolamine, 2nd Class
 98.8Mass content of monoethanolamine, Highest Class, 1st Class

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKAZAN120 / 127439

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.