MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco Rykon® NLGI 1 Premium Grease EP
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Features

Chevron Rykon Premium Grease EP is a high quality, water resistant, extreme pressure, multipurpose lubricating grease.

It is manufactured using highly refined, select high viscosity index base oils, and a polyurea thickener. It is green in color and smooth in texture.

Applications

Chevron Rykon Premium Grease EP is recommended for:

  • automotive applications including heavy duty truck wheel bearings, universal joints, water pumps, and idler pulleys
  • roller bearings operating at 135 to 177ºC (275 to 350ºF) that require a high temperature extreme pressure grease

Chevron Rykon Premium Grease EP is registered with NSF and is acceptable as a lubricant where there is no possibility of food contact (H2) in and around foodprocessing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.

Key Words: CPS Number: 231068; MSDS Number: 7821
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 99Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 787 SUS
Saybolt Viscosity at 210°F 80 SUS
Kinematic Viscosity at 40°C (104°F) 150 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Penetration 277Worked
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -34.0 °C
Dropping Point 260 °C
 
Descriptive Properties
Bearing RustPass
ColorGreen
TextureSmooth
Thickener, % / type12 / Polyurea

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Rykon® 1364 Premium Grease

WCHEV263 / 74878

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.