MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Shakespeare Isocor™ CN30XT Nylon 610
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes: Isocor™ CN30XT is a low viscosity PA-610 based copolymer. This transparent nylon resin is specifically suited for applications requiring increased solvent resistance and UV stability. Isocor™ CN30XT is also used in applications requiring high modulus and low temperature impact properties. This resin can be processed with conventional techniques.

Used for injection molding and film extrusion.

Information provided by Shakespeare Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D 792
Water Absorption 0.28 %24 hour immersion; ASTM D 570
Linear Mold Shrinkage 0.0030 cm/cm
@Thickness 3.17 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9800 psiASTM D 638
Tensile Modulus 333000 psiASTM D 638
Izod Impact, Notched 1.10 ft-lb/inASTM D 256
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 73.0 °CASTM D 3418
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Trogamid® CX9710 Transparent Nylon
EMS-Grivory Grilamid® TR 30 nat PA*
Azoty Tarnow™ Tarnamid® T-27 MTR Polyamide 6 - Transparent
Evonik Trogamid® CX7323 Transparent Nylon
Arkema Rilsamid® AESNO 14 TL PA12

PSHAKE113 / 67392

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.