MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Algoflon® DF 680 F Polytetrafluoroethylene (PTFE)  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Algoflon® DF 680 F is a PFOA-free white fine coagulated powder. It is designed for paste extrusion in medium reduction ratio (RR) range. It is recommended for manufacture of tubes.

Algoflon® DF 680 F shows excellent dimensional stability during processing. The final items exhibit smooth surface and good mechanical properties. They are also more transparent and flexible than those obtained with PTFE homopolymers.

Main features of Algoflon® DF 680 F include:

- Excellent dimensional stability

- Smooth surface

- Good mechanical properties

- Good clarity

Chemical Resistant; Good Processing Stability; Good Thermal Stability; High Clarity; Low Friction

Uses: Aerospace Applications; Automotive Applications; Electrical/Electronic Applications; Industrial Applications; Tubing; Wire & Cable Applications

Availability: Asia Pacific; Europe; North America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.475 g/cc0.0172 lb/in³
Density 2.17 g/cc0.0784 lb/in³ASTM D792
 2.17 g/cc0.0784 lb/in³ASTM D792
Particle Size 550 µm550 µm
 
Descriptive Properties
ColorWhite
FormsPowder

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y6025 / 192946

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.