PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, very low water absorption, and good dimensional stability under severe exposure. 05118 is available in grey. Information supplied by Plenco. |