MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Persian Gulf Polymer LDPE – LD 2420F8
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: LDPE 2420F8 is a non – additive, low density Polyethylene. It is delivered in pellet form. Application: Bags & Pouches, Shopping bags, Sanitary film, Surface protection film. Feature: Homo-polymer, Hygiene grade. Additives: Non Additives.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 - 0.925 g/cc0.0333 - 0.0334 lb/in³ISO 1183 (A)
Melt Flow 0.70 - 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.70 - 0.90 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 21.0 MPa3050 psiISO 527
Film Tensile Strength at Yield, TD 12.0 MPa1740 psiISO 527
Film Elongation at Break, MD >= 200 %>= 200 %ISO 527-1,-3
Film Elongation at Break, TD >= 500 %>= 500 %ISO 527-1,-3
Tensile Impact Strength 28.0 kJ/m²13.3 ft-lb/in²ASTM D4272
Coefficient of Friction 1.01.0ASTM D1894
Tear Strength 30.0 kN/m171 pliTD; ISO 6383-2
 40.0 kN/m228 pliMD; ISO 6383-2
Dart Drop Test >= 140 g>= 0.309 lbASTM D1709
 
Optical PropertiesMetricEnglishComments
Haze 9.0 %9.0 %ASTM D1003 A
Gloss 60 %60 %DIN 67350

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERSI960 / 250364

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.