MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

BASF 3D Ultrafuse® Recycled Polyethylene Terephthalate Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Components: Recycled Polyethylene terephthalate based filament for Fused Filament Fabrication.

Product Description: PET is mainly known by the well-known PET bottle material. This recycled has a natural transparent blueish look. It has excellent 3D printing properties and good mechanical characteristics.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.273 g/cc0.04599 lb/in³Printed Part; ISO 1183-1
Melt Flow 19.2223 g/10 min
@Load 5.00 kg,
Temperature 220 °C
19.2223 g/10 min
@Load 11.0 lb,
Temperature 428 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 14.7 MPa2130 psiZX: Upright; ISO 527
 38.6 MPa5600 psiXY: Flat; ISO 527
Elongation at Break 1.2 %1.2 %ZX: Upright; ISO 527
 4.3 %4.3 %XY: Flat; ISO 527
Modulus of Elasticity 1.334 GPa193.5 ksiYoung's, ZX: Upright; ISO 527
 1.64 GPa238 ksiYoung's, XY: Flat; ISO 527
Flexural Strength 30.2 MPa4380 psiZX: Upright; ISO 178
 65.4 MPa9490 psiXZ: On its edge; ISO 178
 66.9 MPa9700 psiXY: Flat; ISO 178
Flexural Modulus 0.829 GPa120 ksiZX: Upright; ISO 178
 1.551 GPa225.0 ksiXZ: On its edge; ISO 178
 1.662 GPa241.1 ksiXY: Flat; ISO 178
Flexural Strain at Break 3.0 %3.0 %ZX: Upright; ISO 178
 4.8 %4.8 %XZ: On its edge; ISO 178
 5.5 %5.5 %XY: Flat; ISO 178
Izod Impact, Notched (ISO) 1.50 kJ/m²0.714 ft-lb/in²ZX: Upright; ISO 180
 3.30 kJ/m²1.57 ft-lb/in²XZ: On its edge; ISO 180
 4.40 kJ/m²2.09 ft-lb/in²XY: Flat; ISO 180
Izod Impact, Unnotched (ISO) 4.40 kJ/m²2.09 ft-lb/in²ZX: Upright; ISO 180
 21.9 kJ/m²10.4 ft-lb/in²XZ: On its edge; ISO 180
 48.2 kJ/m²22.9 ft-lb/in²XY: Flat; ISO 180
Charpy Impact Unnotched 0.330 J/cm²1.57 ft-lb/in²ZX: Upright; ISO 179-2
 3.37 J/cm²16.0 ft-lb/in²XZ: On its edge; ISO 179-2
 5.55 J/cm²26.4 ft-lb/in²XY: Flat; ISO 179-2
Charpy Impact, Notched 0.100 J/cm²0.476 ft-lb/in²ZX: Upright; ISO 179-2
 0.200 J/cm²0.952 ft-lb/in²XZ: On its edge; ISO 179-2
 0.400 J/cm²1.90 ft-lb/in²XY: Flat; ISO 179-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C160 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 75-2
Glass Transition Temp, Tg 83.0 °C181 °FISO 11357-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 65.0 - 85.0 °C149 - 185 °FBed, Bed Material: Adhesive spray or glue
Nozzle Temperature 225 - 245 °C437 - 473 °F
Drying Temperature 60.0 °C140 °Fin a hot air dryer or vacuum oven
Dry Time 4.00 - 16.0 hour4.00 - 16.0 hour
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Nozzle Diameter=0.4 mm
Print speed30-60 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF3D005 / 312246

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.