MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zircar Ceramics AS-CEM Alumina-Silica Cement
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Type AS-CEM Alumina-Silica Cement is a high temperature resistant cement useful for creating a hard coating on the surfaces of ZIRCAR® Alumina-Silica fibrous ceramic products or other porous insulating Materials. It has useful properties to 1260°C (2300°F).

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 1.54 kV/mm39.0 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.40 µm/m-°C
@Temperature 20.0 °C
3.00 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1260 °C2300 °F
Shrinkage 3.2 %
@Temperature 1260 °C,
Time 86400 sec
3.2 %
@Temperature 2300 °F,
Time 24.0 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 37.2 %37.2 %
Fe2O3 0.70 %0.70 %
MgO 0.30 %0.30 %
Na2O 0.70 %0.70 %
Other 0.60 %0.60 %
SiO2 59.1 %59.1 %
TiO2 1.4 %1.4 %
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials Niobium Carbide (NbC) Coating
Morgan Advanced Ceramics Incronibsi™ Mac-Incronibsi™14-WM Braze Alloy
Morgan Advanced Ceramics Nioro™ ABA Mac-Nioro™ABA-WM Braze Alloy
Morgan Advanced Ceramics Nicusil™ Mac-Nicusil™ 8-WM Braze Alloy
Sandvik Kanthal Super 1900 Molybdenum disilicide

CZIR011 / 2819

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.