MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV 4765B40 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV 4700 Series are very high flow injection molding engineering grades with excellent UV resistance, elasticity, and surface aesthetics designed for demanding automotive applications including window encapsulation and exterior parts. This product is a black, medium hardness, low density thermoplastic vulcanizate suited for injection molding applications that require superior flow properties.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: UV Stabilizer

Features: Chemical Resistant; Good Flexibility; Good Processability; High Flow; High Heat Resistance; Low Compression Set; Low Density; Low Specific Gravity; Medium Hardness

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Window Encapsulation; Rubber Replacement

RoHS Compliance: RoHS Compliant

Automotive Specifications: CHRYSLER MS-AR-100 BMV Color: Black; GM GMN3901 Color: Black; GM GMW15812-TPV(EPDM+PP) Type 5M; GM Sarlink Color: Black; HONDA Unspecified Color: Black

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ISO 1183
Viscosity 230 cP
@Shear Rate 206 1/s,
Temperature 200 °C
230 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  62
@Time 5.00 sec
62
@Time 0.00139 hour
Extruded; ASTM D2240
 65
@Time 5.00 sec
65
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 5.00 MPa725 psiFlow; ASTM D412
 5.60 MPa812 psiAcross Flow; ASTM D412
 4.59 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
666 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 4.93 MPa
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
715 psi
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  2.40 MPa
@Strain 100 %
348 psi
@Strain 100 %
Across Flow; ISO 37
 3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
Flow; ISO 37
 2.35 MPa
@Strain 100 %,
Treatment Temp. 150 °C
341 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
 2.45 MPa
@Strain 100 %,
Treatment Temp. 135 °C
355 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1000 hr; ISO 188
Elongation at Break 360 %360 %Flow; ASTM D412
 490 %490 %Across Flow; ASTM D412
 407 %
@Treatment Temp. 150 °C,
Time 605000 sec
407 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 426 %
@Treatment Temp. 135 °C,
Time 3.60e+6 sec
426 %
@Treatment Temp. 275 °F,
Time 1000 hour
Across Flow, Change in Air; ISO 188
Tear Strength 26.3 kN/m150 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  20 %
@Temperature 22.8 °C,
Time 79200 sec
20 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 26 %
@Temperature 70.0 °C,
Time 79200 sec
26 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 45 %
@Temperature 125 °C,
Time 252000 sec
45 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 232 °C360 - 450 °FInjection
Rear Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Middle Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Front Barrel Temperature 177 - 216 °C350 - 420 °FInjection
Nozzle Temperature 188 - 221 °C370 - 430 °FInjection
Mold Temperature 10.0 - 65.6 °C50.0 - 150 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Screw Speed 100 - 200 rpm100 - 200 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
Teknor Apex Sarlink® TPV 5790B Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV X5750DB Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV X5740DB Thermoplastic Vulcanizate
Teknor Apex Sarlink® TPV X5735B Thermoplastic Vulcanizate

PTEKNQ1163 / 237654

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.