MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

COI Ceramics Nicalon™ HI Type S SiC Ceramic Fiber
Categories: Ceramic; Carbide

Material Notes: Description: A stoichiometric beta-SiC fiber manufactured near-oxygen-free using decarbonization pyrolysis and electron-beam curing. It has higher modulus, creep resistance and oxidation resistance than Hi-Nicalon™. HI-Nicalon™ Type S is highly resistant to oxidation and chemical attack and is available in a variety of product forms, depending on the intended use. The fiber is coated with polyvinyl alcohol (PVA) sizing for improved handleability.

Special Properties: CMC’s reinforced with HI-Nicalon™ Type S ceramic fiber offers distinct advantages over other materials. Oxide fiber and superalloys generally lose mechanical properties above 800C. SiCO fiber generally loses properties above 1000C. 100 micron diameter monofilament SiC fiber is generally not weavable. HI-Nicalon™ Type S ceramic fiber overcomes these drawbacks.

Product Forms:
Continuous Fiber: Supplied as multi-filament tow, spooled on 3 inch ID bobbins to 500 meters in length (100 grams in weight). Also available in random lengths at a reduced price.
Woven Cloth: Available as Plain Weave, 5HS Weave or 8HS Weave, as identified in Table 2, HI-NICALON™ Type S cloth is typically supplied as 30 centimeter-wide continuous rolls of specific lengths. Other widths, weave or braid styles can be made available.
Chopped Fiber: Available as 1-mm length chopped multi-filament tow. Longer lengths also available.

Uses: HI-Nicalon™ Type S ceramic fiber is primarily designed to be used as reinforcement for high temperature ceramic composites. It can also be used as a reinforcement for plastic, and metal matrix composites. Surface treatments are normally recommended to facilitate processing and maximize composite properties. The fiber can also be used to form fibrous products such as high temperature insulation, filters, etc. Its resistance to chemical attack allows the fiber to be used in harsh environments.

Information from COI Ceramics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.10 g/cc0.112 lb/in³
Filament Diameter 12 µm12 µm
Fiber Count 1800 dtex1620 denier
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 2600 MPa377000 psi
Tensile Modulus 420 GPa60900 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.10 ohm-cm0.10 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.10 µm/m-°C
@Temperature 25.0 - 500 °C
2.83 µin/in-°F
@Temperature 77.0 - 932 °F
Specific Heat Capacity  0.700 J/g-°C
@Temperature 25.0 °C
0.167 BTU/lb-°F
@Temperature 77.0 °F
 1.15 J/g-°C
@Temperature 500 °C
0.275 BTU/lb-°F
@Temperature 932 °F
Thermal Conductivity  16.3 W/m-K
@Temperature 500 °C
113 BTU-in/hr-ft²-°F
@Temperature 932 °F
 18.4 W/m-K
@Temperature 25.0 °C
128 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Maximum Service Temperature, Air 1000 °C1830 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 31 %31 %
Oxygen, O 0.20 %0.20 %
Silicon, Si 69 %69 %
 
Descriptive Properties
C/Si Atomic Ratio1.05
Filaments per tow500

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber
Silicon Carbide, CVD
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber
UBE Tyranno Grade SA Ceramic High Temperature Fiber
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator

CCOIC015 / 122055

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.