MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
PolyMirae Moplen EP545L Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen EP545L is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP545L is a heterophasic copolymer typically used by customers in the production of beverage closures using both compression and injection molding technologies. The resin is additivated with both slip and antistatic whilst exhibiting a good stiffness and impact strength. Additional applications for this resin include housewares and medium-sized containers. Moplen EP545L resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for food contact.

Product Features: Good impact and stiffness/Antistatic, Impact Resistance

Typical Applications: Compression & Injection Molded Caps and Closures/Containers/Sports and Leisure/Toys

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 310 kg(f)/cm²ASTM D638
Elongation at Yield 7.0 %ASTM D638
Flexural Modulus 14800 kg(f)/cm²ASTM D790
Izod Impact, Notched 8.00 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyMirae Moplen EP5015 Injection Molding Grade Polypropylene
PolyMirae Moplen EP500M Injection Molding Grade Polypropylene
PolyMirae Moplen EP548P Injection Molding Grade Polypropylene
PolyMirae Adstif HA5034 Injection Molding Grade Polypropylene
PolyMirae Moplen RP343N Injection Molding Grade Polypropylene

PMIRAF25 / 183246

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.