MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ethydco Advancene™ EM-4810-AAH HDPE Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Blow molding. A polymer with broad molecular weight distribution and high molecular weight. This product provides an excellent combination of extrudability and parison stability, which contribute to uniform wall thickness in large parts. It is ideal for blow molding containers of >80 liters closed head shipping containers and other similar parts. The broad distribution also provides outstanding environmental stress crack resistance at a good rigidity. Because of these characteristics, a wide variety of products, such as industrial chemicals, latex paints, printing inks, foodstuffs, adhesives, and other chemical specialties my be packaged in containers produced from this resin. The smooth surface of molded parts is readily treated and printed for high quality applications. Main characteristics: outstanding environmental stress crack resistance, excellent parison melt strength/low sag, good extrudability/processability, good rigidity.

Mechanical property data for samples molded and tested in accordance with ASTM D4976.

Information provided by ETHYDCO.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.948 g/cc0.0342 lb/in³ASTM D792
ESCR 100% Igepal® >= 1500 hour
@Temperature 50.0 °C
>= 1500 hour
@Temperature 122 °F
F50; ASTM D1693
High Load Melt Index 10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
10 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5757ASTM D2240, ISO/IEC 17025:1999
Tensile Strength at Break 36.5 MPa5290 psiASTM D638, ISO 527
Tensile Strength, Yield 22.8 MPa3310 psiASTM D638, ISO 527
Elongation at Break 900 %900 %ASTM D638, ISO 527
Elongation at Yield 6.0 %6.0 %ASTM D638, ISO 527
Flexural Modulus 0.855 GPa124 ksiASTM D790B, ISO 178,
Tensile Impact Strength 462 kJ/m²220 ft-lb/in²Type S; ASTM D1822, ISO 8256
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FASTM D3418, ISO 3146
Crystallization Temperature 114 °C237 °FASTM D3418, ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °C151 °FUnannealed; ASTM D648, ISO 75
Vicat Softening Point 127 °C261 °FASTM D1525, ISO 306
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746, ISO 974( E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Finathene® 50100.3 HDPE blow molding
SCG Chemicals EL-Lene™ H6430BM High Density Polyethylene Blow Molding
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Blow Molding Grade)
LyondellBasell Lupolen 4261 A HDPE, Blow Molding Grade
Formosa Plastics Formolene® HB4903 Blow Molding/Sheet and Thermoforming HDPE

PETHYD901 / 200047

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.