MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Aurora Plastics XP23-45MG PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes: Description: PVC weatherable, integral colored, filled

Application: Body side molding end caps and extruded skin compound which meets Chrysler MSDC 543 and Ford WSK-M4D689-A3

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity <= 1.30 g/cc<= 1.30 g/ccASTM D792, A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 42 - 52
@Time 15.0 sec
42 - 52
@Time 0.00417 hour
ASTM D2240
Tensile Strength >= 12.5 MPa>= 1810 psiType IV, 500mm/min; ASTM D638
Elongation at Break >= 200 %>= 200 %Type IV, 500mm/min; ASTM D638
Tear Strength >= 75.0 kN/m>= 428 pliMethod B; ISO 34
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air -10.0 °C14.0 °FGM9503P
 
Descriptive Properties
Accelerated Weathering<3.0 DEafter 2000 kj/m2, SAEJ2527

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PVC, Molded
Overview of materials for PVC, 10% Glass Fiber Reinforced

PSEPO006 / 140969

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.