MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Proteus™ LSG HS PP-H Heat Stabilized Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Life Science Grade, Heat Stabilized PP-H stock shapes, made from high purity homopolymer polypropylene resin. Shapes are pre-assessed for biocompatibility at the stock shape level (USP VI & ISO 10993) and are supported for use in non-body contact medical applications. Exhibits superior resistance to steam sterilization, cleaning agents, and disinfectants over standard PP materials, and has improved dimensional stability.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 38.0 MPaISO 527-1/-2 (7)
Elongation at Yield 6.00 %ISO 527-1/-2 (7)
Flexural Strength 54.0 MPaISO 178 (12)
Compressive Yield Strength 15.0 MPa
@Strain 1.00 %
ISO 604 (10)
 27.0 MPa
@Strain 2.00 %
ISO 604 (10)
 46.0 MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 6.40 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µin/in-°FASTM E-831 (TMA)
Melting Point 327 °FASTM D3418
Maximum Service Temperature, Air 180 °FContinuous Use Temperature in Air after 20000 hr
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Limited
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Proteus™ HDPE High Density Polyethylene
Mitsubishi Chemical Advanced Materials Proteus™ Homopolymer PP White Polypropylene
Mitsubishi Chemical Advanced Materials Proteus™ LDPE Low Density Polyethylene
Mitsubishi Chemical Advanced Materials Proteus™ Copolymer PP Natural Polypropylene
Aclo Accuguard Polypropylene CP1467V2CSL Copolymer Flame Retardant Copper Stabilized

P1SMP66m / 108908

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.