MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Dow VORAFORCE™ TP 1260/TP 1200/TM 3500 Polyurethane for Composite Systems
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: The VORAFORCE™ TP series consists of formulated systems for pultrusion applications. The VORAFORCE™ TP series of solutions exhibit superior mechanical and thermal properties for a wide range of applications. These systems exhibit low viscosities for efficient fiber wet-out and excellent handling characteristics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1200 - 1400 cP1200 - 1400 cP
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 130 - 140 °C266 - 284 °F
 
Processing PropertiesMetricEnglishComments
Die Temperature 180 - 220 °C356 - 428 °F
Pot Life 25.0 - 35.0 min25.0 - 35.0 min
 
Descriptive Properties
Mix Ratio110 phr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow VORAFORCE™ TL 1651/TL 1600 Polyurethane Glass Composite
Covestro DESMODUR® TT163 + BAYTEC® XL 1705, 93 A Polyurethane, TDI- PTMEG
Dow VORAFORCE™ TJ 1852/TJ 1802/TM 3502 Polyurethane for Composite Systems
Dow TONE™ 0310 Polyol
Dow PELLETHANE® 2104-65D Polyurethane Elastomer (Ether-Ether Hybrid)

PDOW0901 / 185314

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.