MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

EMS-Grivory Grilamid® L 25G nat 6011 Nylon 12, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Mold Release

Features: Food Contact Acceptable; High Viscosity; Lubricated

Uses: Film; Non-oriented Film; Packaging

Agency Ratings: EU Food Contact; FDA Food Contact

RoSH Compliance: RoSH Compliant

Appearance: Natural Color

Forms: Granules

Processing Method: Extrusion; Film Extrusion

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Water Absorption 0.70 %0.70 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 1.5 %1.5 %ISO 62
Water Vapor Transmission 8.07 g/m²/day0.520 g/100 in²/day85% RH; DIS 15106-1/-2
Oxygen Transmission 350 cc-mm/m²-24hr-atm889 cc-mil/100 in²-24hr-atm0% RH; DIS 15105-1/-2
 370 cc-mm/m²-24hr-atm940 cc-mil/100 in²-24hr-atm85% RH; DIS 15105-1/-2
Carbon Dioxide Transmission 1500 cc-mm/m²-24hr-atm3810 cc-mil/100 in²-24hr-atm0% RH; DIS 15105-1/-2
 1600 cc-mm/m²-24hr-atm4060 cc-mil/100 in²-24hr-atm85% RH; DIS 15105-1/-2
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 275 °C
20 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 35.0 MPa5080 psiISO 527-3
Film Tensile Strength at Yield, TD 35.0 MPa5080 psiISO 527-3
Film Elongation at Break, MD 850 %850 %ISO 527-3
Film Elongation at Break, TD 900 %900 %ISO 527-3
Film Elongation at Yield, MD 6.0 %6.0 %ISO 527-3
Film Elongation at Yield, TD 6.0 %6.0 %ISO 527-3
Tensile Modulus 1.60 GPa232 ksiISO 527-1
Tear Strength Test 114114[lbf/in], Trouser, MD; ISO 6383-1
 143143[lbf/in], Trouser, TD; ISO 6383-1
Elmendorf Tear Strength MD 998 g998 gISO 6383-2
Elmendorf Tear Strength TD 998 g998 gISO 6383-2
Film Tensile Strength at Break, MD 80.0 MPa11600 psiISO 527-3
Film Tensile Strength at Break, TD 70.3 MPa10200 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °F10ºC/min; ISO 11357-3
Maximum Service Temperature, Air 110 °C230 °FLong Term; ISO 2578
 150 °C302 °FShort Term
Minimum Service Temperature, Air 80.0 °C176 °FLong Term; ISO 2578
 
Optical PropertiesMetricEnglishComments
Gloss 150 %150 %60°; ISO 2813
 
Descriptive Properties
Gelboflextest1300 holes/m2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRIM076 / 307435

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.