MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

HB Fuller Hydra FAST-EN® DC-12465 Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Description: Hydra FAST-EN ® DC-12465 spray system is a two part spray-able contact adhesive designed to bond higher strength, open cell urethane foams in high stress geometries. It can also be used to bond any open cell urethane foam to a variety of other porous or non-porous surfaces such as other open or closed cell foams, woods, plastics, fabrics and some metals. Hydra FAST-EN ® DC-12465 has aggressive early tack and is solventless, user-friendly and addresses many of the common problems en-countered with other two part systems. Other applications where the use of solvent based, flammable and non-flammable systems are a concern for either health or environmental reasons may al-so be suitable candidates for the use of this product.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccPart A
 1.115 g/cc1.115 g/ccPart B
Solids Content 15 %15 %Part B
 55 %55 %
 55 %55 %Part A
pH 3.53.5Part B
 1212Part A
Storage Temperature 4.44 - 26.7 °C40.0 - 80.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 240 °C464 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 MonthPart A
 12.0 Month12.0 MonthPart B
 
Descriptive Properties
Base compoundPolychloroprenePart A
 Zinc SulfatePart B
ColorBluePart A
 ClearPart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL113 / 316904

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.