MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Trinseo MAGNUM™ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resins are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming processes. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, impact strength and heat properties for use in numerous automotive applications. Melt flow rates from 1 to 12 g/10 min, impact strengths from 2.5 to 12 ft-lb/in and heat distortion temperatures from 165 to 190°F are available. Available primarily as natural plus concentrates, MAGNUM ABS resins are used in a wide variety of automotive applications including structural instrument panels, consoles, pillars, and exterior trim parts requiring painting and plating. MAGNUM 357 HP ABS resin is a medium gloss, high heat material that has slightly higher heat resistance and a little higher melt flow rate than MAGNUM 358 HP ABS resin

Information provided by Styron

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
Melt Density 1.08 g/cc
@Temperature 260 °C
0.0390 lb/in³
@Temperature 500 °F
Maximum Moisture Content 0.100.10
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 2.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
2.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 33.1 MPa4800 psiType I, 51 mm/min; ASTM D638
Tensile Strength, Yield 37.9 MPa5500 psiType I, 51 mm/min; ASTM D638
Elongation at Break 45 %45 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 2.00 GPa290 ksiType I, 51 mm/min; ASTM D638
Flexural Strength 62.1 MPa9010 psiType I, 1.3 mm/min; ASTM D790
Flexural Modulus 2.21 GPa321 ksiType I, 1.3 mm/min; ASTM D790
Izod Impact, Notched  1.30 J/cm
@Thickness 3.20 mm,
Temperature -18.0 °C
2.44 ft-lb/in
@Thickness 0.126 in,
Temperature -0.400 °F
0.25 mm Notch Depth; ASTM D256
 3.10 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
5.81 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm Notch Depth; ASTM D256
Dart Drop, Total Energy  22.6 J
@Thickness 3.20 mm,
Temperature -18.0 °C
16.7 ft-lb
@Thickness 0.126 in,
Temperature -0.400 °F
3.39 m/sec, Peak Energy; ASTM D3763
 23.7 J
@Thickness 3.20 mm,
Temperature -18.0 °C
17.5 ft-lb
@Thickness 0.126 in,
Temperature -0.400 °F
3.39 m/sec, Total Energy; ASTM D3763
 32.8 J
@Thickness 3.20 mm,
Temperature 23.0 °C
24.2 ft-lb
@Thickness 0.126 in,
Temperature 73.4 °F
3.39 m/sec, Peak Energy; ASTM D3763
 42.9 J
@Thickness 3.20 mm,
Temperature 23.0 °C
31.6 ft-lb
@Thickness 0.126 in,
Temperature 73.4 °F
3.39 m/sec, Total Energy; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 81.0 µm/m-°C45.0 µin/in-°FASTM D696
Thermal Conductivity 0.130 W/m-K0.902 BTU-in/hr-ft²-°FMelt; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
@Thickness 3.20 mm
219 °F
@Thickness 0.126 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
@Thickness 3.20 mm
190 °F
@Thickness 0.126 in
Unannealed; ASTM D648
Vicat Softening Point 120 °C248 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 282 °C500 - 540 °F
Mold Temperature 37.8 - 82.2 °C100 - 180 °F
Drying Temperature 82.2 - 85.0 °C180 - 185 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Back Pressure 0.345 - 0.689 MPa50.0 - 99.9 psi
 
Descriptive Properties
Clamp Tonnage2.8-4.1 kN/cm2
Ejection Temperature127°C
No Flow Temperature150°C
Screw Compression Ratio1.5:1 to 3.5:1
Screw L/D Ratio0.834027777777778

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Edinburg Plastics AGA605 ABS
Ravago Manufacturing Americas Hylac® EX28 ABS
LG Chemical HI100 ABS, High Impact
LNP CYCOLOY® MC5510 ABS + PC Alloy
LNP CYCOLOY® MC5513 ABS + PC Alloy

PZZDWST067 / 142276

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.