Aartel 100SD is a new conductive grade developed to dissipate electricity in fuel handling systems. Aartel 100SD maintains all of the excellent properties of general purpose acetal, has a volume resistivity of 5E00 ohm-m, and has an improved resistance to hot diesel fuels. Information provided by Gehrig & Associates |