MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Momentive Performance Materials Silopren™ FFSL 7071 Fully Fluorinated Liquid Silicone Rubber  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding process allows for complex part geometry and exact dimensions. LSR elastomers are generally suitable for short cycle time injection and full automatic flash-less processing. Color pastes are available to pigmenting addition cure productions of LSR's.

All LSR grades are platinum cured materials which are mixed in a 1:1 ratio by weight.

Industries and Applications: The Momentive portfolio of products is used for a wide variety of applications in the Automotive, Aviation and Aerospace, Consumer Goods, Consumer Electronics, Healthcare and Energy Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/cc
Linear Mold Shrinkage 0.027 cm/cm0.027 in/invulcanized 10 sec at 200°C; Without post-cure
 0.035 cm/cm0.035 in/invulcanized 10 sec at 200°C then post-cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6767
Tensile Strength 7.00 MPa1020 psi
Elongation at Break 210 %210 %
Tear Strength 19.0 kN/m108 pliDie B
Compression Set >= 18 %>= 18 %Post cured
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 20.0 °C68.0 °Fcool nozzle and cylinder to prevent premature vulcanization
Mold Temperature 140 - 230 °C284 - 446 °Fshort vulcanization time required (a few seconds)
Injection Pressure 5.00 - 15.0 MPa725 - 2180 psidepends on feed channel
Hold Pressure 5.00 MPa725 psi
 
Descriptive Properties
AppearanceOff White

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials Silopren™ FFSL 7051 Fully Fluorinated Liquid Silicone Rubber
Momentive Performance Materials Silopren™ FFSL 7286/40 Fully Fluorinated Liquid Silicone Rubber
Momentive Performance Materials Silopren™ FFSL 7061 Fully Fluorinated Liquid Silicone Rubber
Momentive Performance Materials Silopren™ FFSL 7041 Fully Fluorinated Liquid Silicone Rubber
Momentive Performance Materials Silopren™ FFSL 7031 Fully Fluorinated Liquid Silicone Rubber

PGE8V793 / 109053

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.